Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM D790 |
NOVA Chemicals Sclair® 56B4 HDPE Blow Molding Resin Extra-high stress crack resistance, Good processabilityApplications: Very high ESCR, Ideally suited for use in most food, pharmaceutical, households and industrial chemical applications, Little/no s.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips HiD® 9035 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM Data |
BASF Capron® 8202C HS Nylon 6 (Conditioned)
(discontinued **) Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | Tangent; ASTM D790 |
Flint Hills P5C4K-089 Random Copolymer Polypropylene Features: Good clarity. Product does not contain animal derived components. Phthalate-freeApplications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Flexural Modulus | 0.972 GPa | 141 ksi | Tangent; ASTM D790 |
Flint Hills P9R6K-054 Random Copolymer Polypropylene Excellent clarity. High flow material. Product does not contain any animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement for PET, .. |
|||
Flexural Modulus | 0.972 GPa | 141 ksi | Tangent; ASTM D790 |
Flint Hills P9R6K-054A Random Copolymer Polypropylene Features: Excellent clarity. High flow material. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement fo.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GV 0350 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ISO 178 |
LyondellBasell Astryn EPF30U Polypropylene Copolymer Key Features: medium melt flow, medium modulus, UV-stabilized, polypropylene copolymer, high impact strength, excellent processabilityApplications: door and luggage compartment scruff plates, seat t.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 55600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Food Pails.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Housewares.. |
|||
Flexural Modulus | 0.975 GPa | 141 ksi | ASTM D790 |
Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at lo.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM Test |
BASF Ultramid® 8202C HS PA6 (Conditioned) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM Test |
BASF Ultramid® 8202C PA6 (Conditioned) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM Test |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Flexural Modulus | 0.970 GPa @Temperature 65.0 °C |
141 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM D790 |
Ashley Polymers Ashlene® 727 Nylon 6 A modified nylon for applications requiring flexibility.Data provided by the manufacturer |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | Secant; ASTM D 790 |
Chevron Phillips LX8124 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 231, A 52600Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, excellent shrinkage resistanceApplic.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® TR-0242-UG MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM Data |
BASF Capron® 1202CQ Nylon 6 (Conditioned)
(discontinued **) Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.970 GPa | 141 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |