Mechanical Properties Metric English Comments
Flexural Modulus 0.920 GPa
133 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers DEXFLEX® 810HSF TPO  (discontinued **)
Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro..
Flexural Modulus 0.920 GPa
133 ksi
1% secant at 0.05 in/min; ASTM D790A
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion
Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance..
Flexural Modulus 0.920 GPa
133 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE
LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated.
Flexural Modulus 0.920 GPa
133 ksi
ISO 178
BASF Nypel® 2351 HS BK PA6 (Dry)
Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6..