Flexural Modulus 2.41 - 6.70 GPa
350 - 972 ksi
Average value: 5.50 GPa Grade Count:11
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..