Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.600 - 4.30 GPa @Temperature -40.0 - 90.0 °C |
87.0 - 624 ksi @Temperature -40.0 - 194 °F |
Average value: 1.92 GPa Grade Count:4 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 0.400 - 4.30 GPa @Temperature -40.0 - 80.0 °C |
58.0 - 624 ksi @Temperature -40.0 - 176 °F |
Average value: 2.14 GPa Grade Count:2 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 1.20 - 4.30 GPa | 174 - 624 ksi | Average value: 2.43 GPa Grade Count:106 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |