Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.3 - 39.2 GPa | 1500 - 5690 ksi | Average value: 16.3 GPa Grade Count:19 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |