Mechanical Properties Metric English Comments
Flexural Modulus 1.42 - 17.9 GPa
206 - 2600 ksi
Average value: 2.49 GPa Grade Count:112
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Flexural Modulus 3.51 - 17.9 GPa
509 - 2600 ksi
Average value: 9.15 GPa Grade Count:31
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Flexural Modulus 4.90 - 17.9 GPa
710 - 2600 ksi
Average value: 10.6 GPa Grade Count:42
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Flexural Modulus 1.10 - 17.9 GPa
160 - 2600 ksi
Average value: 7.09 GPa Grade Count:96
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Flexural Modulus 2.76 - 17.9 GPa
400 - 2600 ksi
Average value: 7.33 GPa Grade Count:131
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..