Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.08 GPa | 1170 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific) LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Flexural Modulus | 8.08 GPa | 1170 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |