Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.53 - 19.0 GPa | 1090 - 2760 ksi | Average value: 11.5 GPa Grade Count:3 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 7.53 GPa | 1090 ksi | ASTM D790 |
Plenco 2424 Phenolic, Granular, Injection Molded