Polymer Property : Flexural Modulus = 7.28 GPa
Polymer Property :
Flexural Modulus =
7.28 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
7.28
GPa
1060
ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP BF004 SAN
LNP* THERMOCOMP* BF004 is a compound based on SAN resin containing 20% Glass Fiber.