Mechanical Properties Metric English Comments
Flexural Modulus 6.24 GPa
905 ksi
ASTM D790
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced
Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Flexural Modulus 6.24 GPa
905 ksi
ISO Value
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
Flexural Modulus 6.24 GPa
905 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12
LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber.
Flexural Modulus 6.24 GPa
905 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12
LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Flexural Modulus 6.24 GPa
905 ksi
ISO 178
Polyplastics Duranex® CN7015 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 6.24 GPa
905 ksi
ISO Value
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista..
Flexural Modulus 6.24 GPa
905 ksi
ISO Value
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional..