Polymer Property : Flexural Modulus = 3.241 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.241 GPa
470.1 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 2005 M 20% Mica Filled Polypropylene
Multi-Pro 2005 M is a mica reinforced polypropylene compound with high stiffness and flex strength. Its high heat resistance lends itself to replace engineered plastics at moderate cost.Data provid..
Flexural Modulus 3.241 GPa
470.1 ksi
ASTM D790
Lucent Polymers TPP-240 Polypropylene, 40% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.