Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.034 GPa | 440.1 ksi | ASTM D790 |
Lucent Polymers TPP-130 Polypropylene, Homopolymer, 30% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |