Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 23.06 GPa | 3345 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding. |