Polymer Property : Flexural Modulus = 2.746 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.746 GPa
398.3 ksi
ASTM D790
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66
Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon.
Flexural Modulus 2.746 GPa

@Temperature 260 °C
398.3 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is..
Flexural Modulus 2.746 GPa

@Temperature 260 °C
398.3 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-G40 ISO 40% Graphite Filled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 car..