Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Nanoblend™ LST 5501 Polypropylene, Unspecified (PP, Unspecified) Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Nymax™ 600 A Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Niche Polymer PA6BK Nylon 6 Information provided by Niche Polymer |
|||
Flexural Modulus | 2.69 - 3.24 GPa | 390 - 470 ksi | ASTM D790 |
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo.. |
|||
Flexural Modulus | 2.69 GPa @Thickness 3.17 mm |
390 ksi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2040ML Nylon 6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Omni Plastics OmniTech™ HPP TF20 V0 Flame Retardant OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 1950 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 6209 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® 930L Nylon 6 (DAM) Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are appli.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-GF10 Natural Homopolymer Polypropylene, 10% Glass Reinforced Information provided by Entec |
|||
Flexural Modulus | 2.69 GPa @Temperature 22.8 °C |
390 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Amco Amalloy® B1172 Polymer Alloy Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Aaron Industries AVPS H 100-3 Virgin Polystyrene Melt flow index may be specified. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-01043 A Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: High Temperature Strength, Impact Modified and LubricatedUL File Number: E157318Information provided by TP C.. |