Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.24 GPa | 325 ksi | Tangent; ASTM D790 |
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 920 PC Opaque colors, low viscosity, superior flame retardance. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 940ASR PC (Asia Pacific) More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 678 ASA Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America F.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Asia Pacific) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips MA5350 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Floppy diskettesDurable household applicationsThin to medium parts that require a combination of high gloss and good toughnessFeatures:Low coeffi.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific) Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.24 - 13.8 GPa | 325 - 2000 ksi | Average value: 7.77 GPa Grade Count:36 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2mm/min; ASTM D790 |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4001HH Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790 |
Clariant Renol SB83642580 ASA Polymer Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | ASTM D790A |
BP Amoco Accpro® 9934 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, Antistatic, High surface hardness, Stain resistanceComplies with FDA specification, Title 21, CFR 177.1520.Typica.. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRPC100 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.24 GPa | 325 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 940 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. |