Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.82 GPa | 2730 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con.. |
|||
Flexural Modulus | 18.82 GPa | 2730 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific) LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond.. |