Polymer Property : Flexural Modulus = 17.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 17.8 GPa
2580 ksi
SGL Carbon Group SIGRAFIL C® filled PEEK
Information provided by SGL Carbon Group
Flexural Modulus 17.8 GPa
2580 ksi
ASTM D790
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
Flexural Modulus 17.8 GPa
2580 ksi
ISO 178
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific)
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 17.8 GPa
2580 ksi
ASTM D790
Unitika RUN35-TA Light resistant PA6, Dry
Light resistant and internalInformation provided by Unitika Ltd.
Flexural Modulus 17.8 GPa
2580 ksi
ISO 178-93
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Flexural Modulus 17.8 GPa
2580 ksi
ISO 178
SABIC Innovative Plastics LNP Verton OV00A PPS
LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.