Polymer Property : Flexural Modulus = 11.66 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 11.66 GPa
1691 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon AE004E ABS
LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region...
Flexural Modulus 11.66 GPa
1691 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific)
LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, ..