Flexural Modulus 1.862 GPa
270.1 ksi
Secant 20% max load; ASTM D-790-95
Multibase Multi-Pro® 3019 CXUW High Gloss 30% TiO2 Filler Content Polypropylene
Multi-Pro 3019 CXUW is a mineral reinforced polypropylene compound exhibiting high stiffness and impact characteristics. This material was specially formulated with UV stabilization for outdoor app..
Flexural Modulus 1.862 GPa
270.1 ksi
RT; ASTM D-790-95
Multibase Multi-ABS 802 Natural Extrusion Grade
Data provided by Multibase.
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and..
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Eastman Tenite Propionate 360E0096907 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, ..
Flexural Modulus 1.862 GPa
270.1 ksi
tangent; ASTM D790
Entec Hypro™ PPH-CC20 Natural Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Information provided by Entec
Flexural Modulus 1.862 GPa
270.1 ksi
tangent; ASTM D790
Entec Hypro™ PPH-T10 Homopolymer Polypropylene, 10% Talc Reinforced
Information provided by Entec
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Diamond Polymers NYLON 6650HSL Black
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Eastman Tenite 360A4861301 Propionate Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.862 GPa
270.1 ksi
ASTM D790
Lucent Polymers TPP-220 Polypropylene, 20% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved