Polymer Property : Flexural Modulus = 1.387 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.387 GPa
201.2 ksi
ASTM D790
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI ..
Flexural Modulus 1.387 GPa
201.2 ksi
ASTM D790
3D Systems DuraForm® PA Nylon for SLS® Systems
For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da..