Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.951 GPa | 138 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | Secant; ISO 178 |
ExxonMobil Exxtral™ BNT 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.Availability: Africa & Middle East, Asia Pacific, E.. |
|||
Flexural Modulus | >= 0.951 GPa | >= 138 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |