Mechanical Properties Metric English Comments
Flexural Modulus 0.686 - 7.11 GPa
99.6 - 1030 ksi
Average value: 2.10 GPa Grade Count:299
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Flexural Modulus 0.686 GPa
99.6 ksi
ASTM D790
Hyosung Topilene C600H PP
C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation
Flexural Modulus 0.686 GPa
99.6 ksi
ASTM D790
Hyosung Topilene C600HF PP
C600HF Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Low sealSlip propertyTransparencyInformation provided by Hyosung Corporation
Flexural Modulus 0.686 GPa

@Thickness 6.40 mm
99.6 ksi

@Thickness 0.252 in
15mm/min; ASTM D790
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Flexural Modulus 0.686 GPa

@Thickness 3.20 mm
99.6 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SC 6501 Toughened Polystyrene
Characteristics Excellent melt strength Extremely tough Easy printability Easy miscibility with most grades of polystyrene Processing Extrusion Thermoforming Injection MoldingApplications Impac..