Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 - 0.827 GPa | 90.0 - 120 ksi | ASTM D790 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Flexural Modulus | 0.621 - 8.27 GPa | 90.0 - 1200 ksi | Average value: 3.90 GPa Grade Count:47 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Modulus | 0.621 GPa | 90.1 ksi | ASTM D790 |
Lucent Polymers TPO-1015 Thermoplastic Polyolefin Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D 790 |
Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer Isocorâ„¢ 653 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ 653 is easily processed and has a wide range of applications due .. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Techmer ES HiFill FR® PP CO FR-N V2 Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8403 Linear Polyethylene for Rotational Molding Borecene RM8403 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-150 BLK288 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-150 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® N100STL (COND, 50% RH) Nylon 6, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300STL (COND, 50% RH) Nylon 6 (Utility Grade), Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100STL (COND, 50% RH) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN200STL (COND, 50% RH) Nylon 66, Super-Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA) HYDLAR® possesses a combination of physical properties that cannot be found in any other commercially available engineered plastic. Design engineers have created a family of superior wear and abra.. |
|||
Flexural Modulus | 0.621 - 1.65 GPa | 90.0 - 240 ksi | Average value: 0.990 GPa Grade Count:88 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 0.621 - 7.24 GPa | 90.0 - 1050 ksi | Average value: 1.79 GPa Grade Count:199 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D3350 |
Formosa Plastics Formolene® HP3902 Pipe HDPE Natural Medium Density Hexene CopolymerApplications: Pipe for gas distribution, oilfield and other industrial pipe, telecommunications conduit.Formolene HP3902 is a high performance copolymer that i.. |