Mechanical Properties Metric English Comments
Flexural Modulus 0.525 GPa
76.1 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static
Nemcon™ E-Series products are designed for use in ESDA electronic assembly environments. E PP AS is a moisture independent anti-static polypropylene characterized by consistent moldability and recy..
Flexural Modulus 0.525 GPa
76.1 ksi
ASTM D790
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass throughout the polyurethane matrix. The composites are 37% to 60% lighter than plywood, d..
Flexural Modulus 0.525 GPa
76.1 ksi
ASTM D790
3M Dyneon™ THV 815GZ Fluorothermoplastic Granules
Dyneon THV 815 GZ provides a balance of low permeation, thermal stability, and melt processability. IT can be used to prepare molded parts and extruded films, tubes, profiles, and wire coatings. It ..