Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.390 GPa | 56.6 ksi | ASTM D790 |
NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin
(discontinued **) Molded Plaque Properties. Features: high flow.Applications: general purpose, housewares.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.390 GPa @Temperature 90.0 °C |
56.6 ksi @Temperature 194 °F |
ASTM D790 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | ASTM D790 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | ASTM D790 |
Ashley Polymers Ashlene® 734-SP5 Nylon 6, Flexible Grade A highly flexible grade of Nylon 6 with outstanding impact.Data provided by the manufacturer |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | ASTM D790 |
Ashley Polymers Ashlene® TD930H Nylon 12 A plasticized Nylon 12 offering outstanding flexibility with superior moisture and chemical resistance, UV and heat stabilized for weatherability.Data provided by the manufacturer |
|||
Flexural Modulus | 0.390 GPa | 56.6 ksi | ASTM D790 |