Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.375 GPa | 54.4 ksi | ASTM D 790 |
NOVA Chemicals Sclair® 72A Butene Copolymer LLDPE Injection Molding Resin 72A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 72A is su.. |
|||
Flexural Modulus | 0.375 GPa @Temperature 65.0 °C |
54.4 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |