Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.325 GPa @Temperature 23.0 °C |
47.1 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |
|||
Flexural Modulus | 0.325 GPa @Temperature 93.0 °C |
47.1 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Flexural Modulus | 0.325 GPa @Temperature 93.0 °C |
47.1 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Flexural Modulus | 0.325 GPa | 47.1 ksi | ASTM D790 |
Reliance Industries Reclair M24300 Polyethylene High flow Linear Low Density Polyethylene grade. Reclair M24300 is butene comonomer based, with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, good fluidity, .. |