Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.211 GPa | 30.6 ksi | 2% Secant; ASTM D 790 |
NOVA Chemicals Novapol® LF-0718-A-INJECTION LDPE Injection Molding Resin LF-0718-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. LF-0718-A is subj.. |
|||
Flexural Modulus | 0.211 GPa | 30.6 ksi | ASTM D790 |
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, High Gloss, Excellent ImpactUses: Large houseware containers, General purpose injection molding |