Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.206 - 0.344 GPa | 29.9 - 49.9 ksi | Secant 1%; ASTM D-790-95 |
Multibase Multi-Flex® TPO 4308 BLK Data provided by Multibase. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 3104-8 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
SK Chemicals SKYPEL G155D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
SK Chemicals SKYPEL M555DH General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ISO 178 |
Chengdu Polyster H605 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent tear resistance. Molded and injected products for consumer use, such as airbag door covers, railwa.. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
Asia Technology Pioneers CAP 102 PP Nanocomposite Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di.. |
|||
Flexural Modulus | 0.206 GPa | 29.9 ksi | ASTM D790 |
SK Chemicals SKYPEL P155D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |