Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.2031 GPa @Temperature 204 °C |
29.46 ksi @Temperature 400 °F |
|
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |