Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0450 GPa | 6.53 ksi | ISO 178 |
Polimeri Europa Clearflex® MQ F0 Very Low Density Polyethylene Clearflex MQ F0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Flexural Modulus | 0.0450 GPa @Temperature 49.0 °C |
6.53 ksi @Temperature 120 °F |
ASTM D790 |
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | ISO 178 |
Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H3303 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl.. |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MV 3000 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 3000 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on .. |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on .. |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | ASTM D638 |
Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional group.. |
|||
Flexural Modulus | 0.0450 - 0.115 GPa | 6.53 - 16.7 ksi | Average value: 0.0733 GPa Grade Count:3 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Modulus | 0.0450 GPa | 6.53 ksi | ASTM D638 |
Arkema Group LOTRYL® 17 BA 04 Copolymer Ethylene - Butyl Acrylate LOTRYL® 17 BA 04 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 17 BA 04 is used as tie layer in coextrusion PP/PE, for extrusi.. |