Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0414 GPa | 6.00 ksi | Procedure B, 0.05 in/min; ASTM D790 |
S&E Specialty Polymers TufTech™ 12-041 PVC Compound Application: A PVC based semi-rigid compound designed for general purpose use in extruded form, including piping applications.Information provided by S&E Specialty Polymers |
|||
Flexural Modulus | 0.0414 GPa | 6.00 ksi | ASTM D790 |
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Flexural Modulus | 0.0414 GPa | 6.00 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® UL 7520 Adhesive Application Resin Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealan.. |
|||
Flexural Modulus | 0.0414 GPa | 6.00 ksi | 1% secant; ASTM D-790 |
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane
(discontinued **) Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En.. |