Flexural Modulus 0.0386 GPa
5.60 ksi
ASTM D790
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Flexural Modulus 0.0386 GPa
5.60 ksi
ASTM D790
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol