Mechanical Properties Metric English Comments
Flexural Modulus 0.0260 GPa
3.77 ksi
ASTM D790
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca..
Flexural Modulus 0.0260 GPa
3.77 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-760 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Ap..
Flexural Modulus 0.0260 - 12.4 GPa
3.77 - 1800 ksi
Average value: 1.44 GPa Grade Count:725
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Flexural Modulus 0.0260 GPa
3.77 ksi
ASTM D790
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0260 GPa
3.77 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved