Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.406 J/cm

@Thickness 12.7 mm
0.760 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP610 Paper Base Laminate
Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne..
Izod Impact, Unnotched 0.406 J/cm

@Thickness 12.7 mm
0.760 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP612 Paper Base Laminate
Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require..