Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.07 J/cm @Thickness 12.7 mm |
2.00 ft-lb/in @Thickness 0.500 in |
LW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315. |
|||
Izod Impact, Unnotched | 1.07 J/cm @Thickness 12.7 mm |
2.00 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP318 Cotton Fabric Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t.. |