Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.90 GPa @Temperature 80.0 °C |
1150 ksi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 7.93 GPa @Temperature 177 °C |
1150 ksi @Temperature 351 °F |
Autoclave Cured; [90°]16 |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |