Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.70 GPa @Temperature 232 °C |
1120 ksi @Temperature 450 °F |
T300 (6K); [90°]16 |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |