Polymer Property : Flexural Modulus = 142.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 142.7 GPa

@Temperature 232 °C
20700 ksi

@Temperature 450 °F
T300 (6K); [0°]16
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel