Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 5.01 J @Temperature -30.0 °C |
3.69 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |