Polymer Property : Dart Drop, Total Energy = 49.4 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 67.0 J

@Temperature -30.0 °C
49.4 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 67.0 J

@Temperature -30.0 °C
49.4 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 67.0 J

@Temperature -28.9 °C
49.4 ft-lb

@Temperature -20.0 °F
ASTM D3763
Styron Pulse® 2000 ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.