Polymer Property : Dart Drop, Total Energy = 18.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 24.4 J

@Temperature -40.0 °C
18.0 ft-lb

@Temperature -40.0 °F
ASTM D3736
ExxonMobil Escorene® UL 7765 Adhesive Application Resin
Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t..
Dart Drop, Total Energy 24.4 J

@Temperature -40.0 °C
18.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A..
Dart Drop, Total Energy 24.4 J

@Temperature -20.0 °C
18.0 ft-lb

@Temperature -4.00 °F
ASTM D3763
ExxonMobil LD 506.07 Compounding and molding resin
Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit..
Dart Drop, Total Energy 24.4 J

@Temperature -20.0 °C
18.0 ft-lb

@Temperature -4.00 °F
ASTM D3763
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin
Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit..