Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 66.0 MPa @Temperature 760 °C, Time 36000 sec |
9570 psi @Temperature 1400 °F, Time 10.0 hour |
Typical Stress-Rupture |
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Rupture Strength | 66.0 MPa @Temperature 700 °C, Time 3.60e+7 sec |
9570 psi @Temperature 1290 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 25Cr/12Ni No. HR7 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |