Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 46.0 MPa @Temperature 870 °C, Time 360000 sec |
6670 psi @Temperature 1600 °F, Time 100 hour |
Initial Stress |
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Rupture Strength | 46.0 MPa @Temperature 750 °C, Time 3.60e+7 sec |
6670 psi @Temperature 1380 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 25Cr/12Ni No. HR7 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Rupture Strength | 46.0 MPa @Temperature 980 °C, Time 360000 sec |
6670 psi @Temperature 1800 °F, Time 100 hour |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |