Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 185 MPa @Temperature 650 °C, Time 36000 sec |
26800 psi @Temperature 1200 °F, Time 10.0 hour |
Typical Stress-Rupture |
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |