Mechanical Properties Metric English Comments
Rupture Strength 18.0 MPa

@Temperature 850 °C,
Time 3.60e+7 sec
2610 psi

@Temperature 1560 °F,
Time 10000 hour
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Rupture Strength 18.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
2610 psi

@Temperature 1470 °F,
Time 10000 hour
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Rupture Strength 18.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
2610 psi

@Temperature 1470 °F,
Time 10000 hour
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Rupture Strength 18.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
2610 psi

@Temperature 1470 °F,
Time 10000 hour
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Rupture Strength 18.0 MPa

@Temperature 950 °C,
Time 3.60e+7 sec
2610 psi

@Temperature 1740 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 37Ni/18Cr/Nb No. HR32
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..