Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 138 MPa | 20000 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Hardness, H358/30 | 138 MPa | 20000 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Hardness, H358/30 | 138 MPa | 20000 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Hardness, H358/30 | 138 MPa | 20000 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Hardness, H358/30 | 138 MPa | 20000 psi | ISO 2039-1 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Hardness, H358/30 | 138 MPa | 20000 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |