Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 70.0 MPa | 10200 psi | ISO 2039-1 |
SABIC Innovative Plastics GELOY CR7020 ASA (Europe-Africa-Middle East) GELOY CR7020 is a profile extrusion and co-extrusion grade, blend of ASA/SAN. In co-extrusion it can be used over CYCOLAC, PVC or other compatible polymers. |
|||
Hardness, H358/30 | 70.0 MPa | 10200 psi | ISO 2039-1 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Hardness, H358/30 | 70.0 MPa | 10200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East) NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive |
|||
Hardness, H358/30 | 70.0 MPa | 10200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PX1180 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1180 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a.. |
|||
Hardness, H358/30 | 70.0 MPa | 10200 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PX1181 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1181 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a .. |
|||
Hardness, H358/30 | 70.0 MPa | 10200 psi | ISO 2039-1 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |