Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 166 MPa | 24100 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |